How many detonators are planted during protection of track for welding site ?
(i) One
(ii) Two
(iii) Three*
(iv) None of the above

1 Answer

Answer :

iii) Three*

Related questions

Description : Weather protection of track is required during block for execution of AT Welding? (i) Yes.* (ii) No (iii) As decided by site supervisor (iv) As per site condition

Last Answer : (i) Yes.*

Description : Ist detonator is planted at a distance of (i) 1200 Mt. from welding site .* (ii) 600 mtrs from welding site (iii) 30 mtrs from welding site (iv) None of the above

Last Answer : (i) 1200 Mt. from welding site .*

Description : Banner flag is planted at a distance of (i) At the site of work (ii) At 1200 mtrs from welding site (iii) At 30 mtrs from welding site (iv) 600 Mt. from welding site .*

Last Answer : iv) 600 Mt. from welding site .

Description : Last flag man is deputed at which distance from last detonator during protection of welding site . (i) 30 mts (ii) 50 mts (iii) 45 (iv) 60 mts

Last Answer : (iv) 60 mts

Description : Distance between the two detonators should be (i) 15 Mt. (ii) 10 Mt.* (iii) 20 Mt (iv) None of the above

Last Answer : (ii) 10 Mt.*

Description : Weather date of welding is marked on weld? (i) Yes (ii) As decided by the site supervisor (iii) No* (iv) None of the above

Last Answer : (iii) No*

Description : Which gauge is used to measure the height of rail at the time of aligning of rails for AT welding? (i) Height gauge.* (ii) Vertical gauge (iii) Horizontal gauge (iv) As decided by site supervisor

Last Answer : (iv) As decided by site supervisor

Description : Weather traffic block is required for execution of AT Welding? (i) Yes.* (ii) No (iii) As decided by site supervisor (iv) As per site condition

Last Answer : (i) Yes.

Description : For protection of level crossing gate in an emergency on BG double line the Gateman should place one detonator at one place and 3 detonators at a subsequent place at a distance of ------- a) and------ ... c) 500 meters and 1000 meters d) 600 meters and 1200 meters* e) 800 meters in 1500 meters

Last Answer : d) 600 meters and 1200 meters*

Description : Name the material which is separated from molten steel during chemical reaction of A.T welding? (i) Aluminium oxide (slag). * (ii) Ferrous Oxide (iii) Aluminium (iv) Ferrous

Last Answer : (i) Aluminium oxide (slag). *

Description : During AT welding reaction is ? (i) Exothermic .* (ii) Endothermic (iii) No Reaction (iv) Heating

Last Answer : (i) Exothermic .*

Description : Type of competency certificate issued after TW-1 course? (i) Competency for two years (ii) Provisional competency.* (iii) Competency for six months (iv) Competency to do welding independently

Last Answer : (ii) Provisional competency.*

Description : If code of a fracture is OFW-422 then it means. (i) AT welding with transverse crack. (ii) Flash butt welding with transverse crack. (iii) At welding with horizontal crack.* (iv) None of the above.

Last Answer : (iii) At welding with horizontal crack.*

Description : In AT welding process what is the role of asbestos powder & slag ? (i) To separate closing pin from portion* (ii) To hold the portion (iii) Both above are correct (iv) None of the above

Last Answer : (i) To separate closing pin from portion*

Description : In AT welding process what is the role of closing pin ? (i) To hold the portion before melt (ii) To hold the asbestos powder & slag (iii) Both above are correct* (iv) None of the above

Last Answer : (iii) Both above are correct*

Description : What is the testing frequency of new AT weld ? (i) Just after the welding (ii) After 7 days of welding (iii) With in the one month of welding* (iv) None of the above

Last Answer : iii) With in the one month of welding*

Description : In how many time final grinding should be done of new AT weld ? (i) Just after the welding (ii) After 8 hrs of welding (iii) With in 24 hrs* (iv) None of the above

Last Answer : iii) With in 24 hrs*

Description : In how many time rough riding should be done of new AT weld ? (i) Just after the welding* (ii) After 8 hrs of welding (iii) After 24 hrs (iv) None of the above

Last Answer : i) Just after the welding*

Description : Rails used for A T Welding shall not normally be welded? (i) 20 years old . (ii) 30 years old (iii) 40 years old (iv) 50 years old*

Last Answer : iv) 50 years old*

Description : Name the paint used in A.T. Welding painting? (i) Black Paint (ii) Bituminous black IS:9862-1981.* (iii) Any type of black paint (iv) None of the above

Last Answer : (ii) Bituminous black IS:9862-1981.*

Description : When was the collar painting done ? (i) After the welding * (ii) after one week of welding (iii) After 15 days of welding (iv) None of the above

Last Answer : (i) After the welding *

Description : What will happen if slag is not used above the layer of asbestos powder? (i) Auto tapping* (ii) High welding (iii) Low welding (iv) Nothing will happen

Last Answer : (i) Auto tapping*

Description : After AT Welding First train is to be passed after ? (i) 20 Minutes from pouring of weld metal. (ii) 35 Minutes from pouring of weld metal. (iii) 30 Minutes from pouring of weld metal.* (iv) 25 Minutes from pouring of weld metal.

Last Answer : (iii) 30 Minutes from pouring of weld metal.*

Description : What are the recognized systems for pre heating of rails ends for AT Welding? (i) Oxygen –LPG & Compressed air petrol both* (ii) Only Oxygen –LPG (iii) Only Compressed air petrol both (iv) both are correct

Last Answer : ) Oxygen –LPG & Compressed air petrol both*

Description : What is Pre Heating Temperature of rail ends in AT Welding? (i) 300 ± 20oC (ii) 400 ± 20oC (iii) 500 ± 20oC (iv) 600 ± 20oC *

Last Answer : (iv) 600 ± 20oC *

Description : Where Portion sample tests(test piece) should be conducted? (i) At desire by RDSO (ii) At Zonal CMT’s organisation or the Flash Butt Welding plant. * (iii) In RDSO campus (iv) As decided by in charge of the plant

Last Answer : At Zonal CMT’s organisation or the Flash Butt Welding plant.

Description : How rejected portion are to be disposed-off? (i) By Igniting 5 Portions at a time in pit away from store?* (ii) By throwing them away (iii) By dispose off in a pit (iv) By using it in Branch/Yard lines for welding

Last Answer : (i) By Igniting 5 Portions at a time in pit away from store?*

Description : In new Rail as well as second hand rails how much end bends of the rails in vertical are permitted when checked with one meter straight edge before welding? (i) +0.5mm, -0 mm in vertical * (ii) +0.2mm, -.3 mm in vertical (iii) +0.3mm, -2 mm in vertical (iv) 0 mm, +.5 mm in vertical

Last Answer : (i) +0.5mm, -0 mm in vertical *

Description : hat is the minimum distance between AT Weld and other joint exist in track? (i) 2 Mt. (ii) 3 Mt. (iii) 4 Mt.* (iv) 4.5 Mt.

Last Answer : (iii) 4 Mt.*

Description : Normal life of detonators is e. 5 years f. 10 years g. 7 years * h. 6 years.

Last Answer : g. 7 years *

Description : Thickness of Lining/Charge is kept? (i) 20 mm. (ii) 25 mm* (iii) 30 mm (iv) As decided by the site supervisor

Last Answer : (ii) 25 mm*

Description : How much rail ends are cleaned with Kerosene Oil and steel wire brush? (i) Minimum 100 mm both side (ii) Minimum 50 mm both side.* (iii) No need (iv) As decided by site supervisor

Last Answer : (ii) Minimum 50 mm both side.*

Description : In new Rail as well as second hand rails how much end bends of the rails in lateral direction are permitted when checked with one metre straight edge before welding? (i) ± 0.2 mm in lateral direction (ii) ± 0.3 mm in lateral direction (iii) ± 0.5 mm in latera

Last Answer : (iii) ± 0.5 mm in latera

Description : During periodic testing of an AT weld with 700 probe, a bunch of moving signals of less than 40% but more than 10% is observed in the head of weld, the joint will be. (i) Good joint.* (ii) DFWR (iii) DFWO (iv) OBSW

Last Answer : i) Good joint.*

Description : For rolling mark 60 kg/Sail/X/2010 the first testing in the field after initial testing of rails in rail manufacturing plant, will be done. (i) After test free period of 25%. (ii) After passage of every 40 ... period.* (iii) After passage of 200 GMT. (iv) On the basis of annual GMT of the section.

Last Answer : (ii) After passage of every 40 GMT traffic during test free period.*

Description : Defect of High joint is due to ? (i) Early trimming of weld (ii) Excess provision of height during alignment.* (iii) Early grinding of weld (iv) None of above

Last Answer : (ii) Excess provision of height during alignment.

Description : Defect of low joint is due to? (i) Excess height (ii) Early trimming of weld (iii) Early grinding of weld (iv) Nil/Less provision of height during alignment.

Last Answer : (iv) Nil/Less provision of height during alignment.

Description : Pressure of Oxygen during pre-heating shall be? (i) 4.0 – 5.0 kg/ sq cm (ii) 5.0 – 6.0 kg/ sq cm (iii) 6.0 – 7.0 kg/ sq cm (iv) 7.0 – 8.0 kg/ sq cm *

Last Answer : (iv) 7.0 – 8.0 kg/ sq cm *

Description : ressure of LPG during pre-heating shall be? (i) 2.0 - 2.5 kg/ sq cm (ii) 2.0 - 2.5 kg/ sq cm (iii) 2.0 - 2.5 kg/ sq cm* (iv) 2.0 - 2.5 kg/ sq cm

Last Answer : (iii) 2.0 - 2.5 kg/ sq cm*

Description : Min. breaking load of 60kg weld during transverse breaking load test is? (i) 110 MT (ii) 115 MT* (iii) 90 MT (iv) 120 MT

Last Answer : (ii) 115 MT*

Description : Min. breaking load of 52kg weld during transverse breaking load test is? (i) 90MT* (ii) 100 MT (iii) 110 MT (iv) 120 MT

Last Answer : (i) 90MT*

Description : Minm. deflection during transverse breaking load test is? (i) 5 mm (ii) 10 mm (iii) 15 mm* (iv) 20 mm

Last Answer : (iii) 15 mm*

Description : Pressure of compressed air is kept during preheating by CAPS? (i) 1 to 2 kg/cm2 (ii) .1 to .2 kg/cm2 (iii) 2 to 3 kg/cm2 (iv) 0.2 to 0.3 kg/cm2*

Last Answer : (iv) 0.2 to 0.3 kg/cm2*

Description : Marking of DFWO weld is. (i) Two red point circle on both faces of weld.* (ii) Two red point cross on both faces of weld. (iii) One red point circle on both faces of weld. (iv) None of the above.

Last Answer : i) Two red point circle on both faces of weld.*

Description : After declare good in USFD testing what is the joggling criteria ? (i) Joggle will be open from the AT weld* (ii) Joggling with two far end bolting (iii) joggling with four tight bold (iv) None of the above

Last Answer : (i) Joggle will be open from the AT weld*

Description : Till USFD testing of new AT weld what is criteria for joggling ? (i) Joggling with two far end bold (ii) Joggling with two tight clamps* (iii) Leave without joggling till its testing (iv) None of the above

Last Answer : (ii) Joggling with two tight clamps*

Description : What is the validity after Refresher course for welders (TW-2)? (i) Six monyhs (ii) One year (iii) Two years.* (iv) All are wrong

Last Answer : (iii) Two years.*

Description : What is the duration for supervisors course (TW-3)? (i) One week * (ii) Two weeks (iii) As decided by TPP/LKO (iv) 3 working days

Last Answer : (i) One week

Description : What is the duration for Refresher course for welders (TW-2)? (i) One week* (ii) Two weeks (iii) As decided by TPP/LKO (iv) 3 working days

Last Answer : (i) One week*

Description : What is the duration for Initial course for welders (TW-1)? (i) Two weeks* (ii) One week (iii) As decided by TPP/LKO (iv) 3 working days

Last Answer : (i) Two weeks*