Rails used for A T Welding shall not normally be welded?
(i) 20 years old .
(ii) 30 years old
(iii) 40 years old
(iv) 50 years old*

1 Answer

Answer :

iv) 50 years old*

Related questions

Description : Which gauge is used to measure the height of rail at the time of aligning of rails for AT welding? (i) Height gauge.* (ii) Vertical gauge (iii) Horizontal gauge (iv) As decided by site supervisor

Last Answer : (iv) As decided by site supervisor

Description : What are the recognized systems for pre heating of rails ends for AT Welding? (i) Oxygen –LPG & Compressed air petrol both* (ii) Only Oxygen –LPG (iii) Only Compressed air petrol both (iv) both are correct

Last Answer : ) Oxygen –LPG & Compressed air petrol both*

Description : In new Rail as well as second hand rails how much end bends of the rails in vertical are permitted when checked with one meter straight edge before welding? (i) +0.5mm, -0 mm in vertical * (ii) +0.2mm, -.3 mm in vertical (iii) +0.3mm, -2 mm in vertical (iv) 0 mm, +.5 mm in vertical

Last Answer : (i) +0.5mm, -0 mm in vertical *

Description : The increased gain of 10 dbs for single line & ‘D’ marks rails on double/multiple lines shall be employed for classification of defects. (i) defect in weld (ii) defects in rail. * (iii) for both defects on weld & rail. (iv) None of above.

Last Answer : ii) defects in rail. *

Description : What is the validity after supervisors course (TW-3)? (i) Normally, supervisors shall not be required to undergo the course again. However, they may be sent for course on performance basis.* (ii) 2 years (iii) 5 Years (iv) 10 Years

Last Answer : (i) Normally, supervisors shall not be required to undergo the course again. However, they may be sent for course on performance basis.*

Description : Last flag man is deputed at which distance from last detonator during protection of welding site . (i) 30 mts (ii) 50 mts (iii) 45 (iv) 60 mts

Last Answer : (iv) 60 mts

Description : For rolling mark 60 kg/Sail/X/2010 the first testing in the field after initial testing of rails in rail manufacturing plant, will be done. (i) After test free period of 25%. (ii) After passage of every 40 ... period.* (iii) After passage of 200 GMT. (iv) On the basis of annual GMT of the section.

Last Answer : (ii) After passage of every 40 GMT traffic during test free period.*

Description : After AT Welding First train is to be passed after ? (i) 20 Minutes from pouring of weld metal. (ii) 35 Minutes from pouring of weld metal. (iii) 30 Minutes from pouring of weld metal.* (iv) 25 Minutes from pouring of weld metal.

Last Answer : (iii) 30 Minutes from pouring of weld metal.*

Description : Painting of weld is done up to (i) 10 CM minimum both side of weld & on welded surface .* (ii) 15 CM minimum both side of weld & on welded surface (iii) 20 CM minimum both side of weld & on welded surface (iv) None of the above

Last Answer : (i) 10 CM minimum both side of weld & on welded surface .*

Description : In new Rail as well as second hand rails how much end bends of the rails in lateral direction are permitted when checked with one metre straight edge before welding? (i) ± 0.2 mm in lateral direction (ii) ± 0.3 mm in lateral direction (iii) ± 0.5 mm in latera

Last Answer : (iii) ± 0.5 mm in latera

Description : Name the paint used in A.T. Welding painting? (i) Black Paint (ii) Bituminous black IS:9862-1981.* (iii) Any type of black paint (iv) None of the above

Last Answer : (ii) Bituminous black IS:9862-1981.*

Description : Name the material which is separated from molten steel during chemical reaction of A.T welding? (i) Aluminium oxide (slag). * (ii) Ferrous Oxide (iii) Aluminium (iv) Ferrous

Last Answer : (i) Aluminium oxide (slag). *

Description : Height of crucible is kept from top surface of mould? (i) 30 mm (ii) 40 mm (iii) 50 mm* (iv) 60 mm

Last Answer : (iii) 50 mm*

Description : Ist detonator is planted at a distance of (i) 1200 Mt. from welding site .* (ii) 600 mtrs from welding site (iii) 30 mtrs from welding site (iv) None of the above

Last Answer : (i) 1200 Mt. from welding site .*

Description : Banner flag is planted at a distance of (i) At the site of work (ii) At 1200 mtrs from welding site (iii) At 30 mtrs from welding site (iv) 600 Mt. from welding site .*

Last Answer : iv) 600 Mt. from welding site .

Description : Type of competency certificate issued after TW-1 course? (i) Competency for two years (ii) Provisional competency.* (iii) Competency for six months (iv) Competency to do welding independently

Last Answer : (ii) Provisional competency.*

Description : What is the time of removal the tensor from the newly executed A T Weld? (i) 15 minutes after pouring. (ii) 20 minutes after pouring* (iii) 25 minutes after pouring. (iv) 30 minutes after pouring.

Last Answer : (ii) 20 minutes after pouring*

Description : Addition gain of 10 db is used for testing. (i) ‘D’ marked rails on single lines. (ii) ‘D’ marked rails on double lines. (iii) Testing on single line and ‘D’ marked rails on double/multiple lines section.* (iv) None of above.

Last Answer : (iii) Testing on single line and ‘D’ marked rails on double/multiple lines section.*

Description : To take care of differential cooling rail ends of 72 UTS rails are lifted by? (i) 1 to 1.5 mm (ii) 1 to 2 mm (iii) 2 to 2.5 mm (iv) 3 to 4 mm *

Last Answer : iv) 3 to 4 mm *

Description : To take care of differential cooling rail ends of 90 UTS rails are lifted by? (i) 1 mm (ii) 2 mm (iii) 2 to 2.2 mm.* (iv) 1 to 2 mm

Last Answer : (iii) 2 to 2.2 mm.*

Description : In case of Shot Welded Rails the fish plated joint should be avoided on Level Crossings within a distance of --------- from end of level crossing a) 3 meters b) 4 meters c) 5 meters d) 6 meters*

Last Answer : d) 6 meters*

Description : If code of a fracture is OFW-422 then it means. (i) AT welding with transverse crack. (ii) Flash butt welding with transverse crack. (iii) At welding with horizontal crack.* (iv) None of the above.

Last Answer : (iii) At welding with horizontal crack.*

Description : In AT welding process what is the role of asbestos powder & slag ? (i) To separate closing pin from portion* (ii) To hold the portion (iii) Both above are correct (iv) None of the above

Last Answer : (i) To separate closing pin from portion*

Description : In AT welding process what is the role of closing pin ? (i) To hold the portion before melt (ii) To hold the asbestos powder & slag (iii) Both above are correct* (iv) None of the above

Last Answer : (iii) Both above are correct*

Description : What is the testing frequency of new AT weld ? (i) Just after the welding (ii) After 7 days of welding (iii) With in the one month of welding* (iv) None of the above

Last Answer : iii) With in the one month of welding*

Description : In how many time final grinding should be done of new AT weld ? (i) Just after the welding (ii) After 8 hrs of welding (iii) With in 24 hrs* (iv) None of the above

Last Answer : iii) With in 24 hrs*

Description : In how many time rough riding should be done of new AT weld ? (i) Just after the welding* (ii) After 8 hrs of welding (iii) After 24 hrs (iv) None of the above

Last Answer : i) Just after the welding*

Description : How many detonators are planted during protection of track for welding site ? (i) One (ii) Two (iii) Three* (iv) None of the above

Last Answer : iii) Three*

Description : Weather date of welding is marked on weld? (i) Yes (ii) As decided by the site supervisor (iii) No* (iv) None of the above

Last Answer : (iii) No*

Description : When was the collar painting done ? (i) After the welding * (ii) after one week of welding (iii) After 15 days of welding (iv) None of the above

Last Answer : (i) After the welding *

Description : What will happen if slag is not used above the layer of asbestos powder? (i) Auto tapping* (ii) High welding (iii) Low welding (iv) Nothing will happen

Last Answer : (i) Auto tapping*

Description : Weather traffic block is required for execution of AT Welding? (i) Yes.* (ii) No (iii) As decided by site supervisor (iv) As per site condition

Last Answer : (i) Yes.

Description : Weather protection of track is required during block for execution of AT Welding? (i) Yes.* (ii) No (iii) As decided by site supervisor (iv) As per site condition

Last Answer : (i) Yes.*

Description : What is Pre Heating Temperature of rail ends in AT Welding? (i) 300 ± 20oC (ii) 400 ± 20oC (iii) 500 ± 20oC (iv) 600 ± 20oC *

Last Answer : (iv) 600 ± 20oC *

Description : During AT welding reaction is ? (i) Exothermic .* (ii) Endothermic (iii) No Reaction (iv) Heating

Last Answer : (i) Exothermic .*

Description : Where Portion sample tests(test piece) should be conducted? (i) At desire by RDSO (ii) At Zonal CMT’s organisation or the Flash Butt Welding plant. * (iii) In RDSO campus (iv) As decided by in charge of the plant

Last Answer : At Zonal CMT’s organisation or the Flash Butt Welding plant.

Description : How rejected portion are to be disposed-off? (i) By Igniting 5 Portions at a time in pit away from store?* (ii) By throwing them away (iii) By dispose off in a pit (iv) By using it in Branch/Yard lines for welding

Last Answer : (i) By Igniting 5 Portions at a time in pit away from store?*

Description : Thickness of Lining/Charge is kept? (i) 20 mm. (ii) 25 mm* (iii) 30 mm (iv) As decided by the site supervisor

Last Answer : (ii) 25 mm*

Description : DFWR weld shall be replaced. (i) Within 2 months of detection. (ii) Within 1 year of detection. (iii) Within 3 months of detection.* (iv) after 3 days of detection.

Last Answer : (iii) Within 3 months of detection.*

Description : Sensitivity calibration against temp. variation shall be carried out. (i) At least once in month* (ii) quarterly. (iii) at least once in six months (iv) Any of above.

Last Answer : i) At least once in month*

Description : What is the speed restriction to be observed for train passing? (i) Necessary speed restriction shall be observed until the grinding operation is over.* (ii) 30KMPH (iii) 45 KMPH (iv) Not required

Last Answer : (i) Necessary speed restriction shall be observed until the grinding operation is over.*

Description : Pressure of Oxygen during pre-heating shall be? (i) 4.0 – 5.0 kg/ sq cm (ii) 5.0 – 6.0 kg/ sq cm (iii) 6.0 – 7.0 kg/ sq cm (iv) 7.0 – 8.0 kg/ sq cm *

Last Answer : (iv) 7.0 – 8.0 kg/ sq cm *

Description : ressure of LPG during pre-heating shall be? (i) 2.0 - 2.5 kg/ sq cm (ii) 2.0 - 2.5 kg/ sq cm (iii) 2.0 - 2.5 kg/ sq cm* (iv) 2.0 - 2.5 kg/ sq cm

Last Answer : (iii) 2.0 - 2.5 kg/ sq cm*

Description : Finished tolerance on 10 cm. long st. edge on surface of head shall be? (i) 0 to 0.1 mm (ii) 0 to 0.2 mm (iii) 0 to 0.4 mm* (iv) 0 to 0.3 mm

Last Answer : (iii) 0 to 0.4 mm*

Description : Finished tolerance on 10 cm long st. edge at the centre on gauge side shall be? (i) ± 0.4 mm (ii) ± 0.1 mm (iii) ± 0.2 mm (iv) ± 0.3 mm*

Last Answer : iv) ± 0.3 mm*

Description : Finished tolerance on 1 Mt. long st. edge on surface of head shall be? (i) 0 to .1 mm (ii) 1 to 1.5 mm (iii) 0 mm (iv) 0 to 1 mm*

Last Answer : (iv) 0 to 1 mm*

Description : Finished tolerance on 1 Mt. st. edge at the centre on gauge side shall be? (i) ± 0.2 mm (ii) ± 0.3 mm (iii) ± 0.5 mm* (iv) ± 1.0 mm

Last Answer : (iii) ± 0.5 mm*

Description : Rails in the field are generally welded by using a) Thermit welding b) Gas welding c) Electric arc welding d) Forge welding

Last Answer : a) Thermit welding

Description : Check rails should normally be provided where the radius is …. M or less in B.G. (a) 150m (b) 200m (c) 218m* (d) 240m

Last Answer : (c) 218m*

Description : Check rails should normally be provided where the radius is ……. M or less in B.G. (a) 150m (b) 200m (c) 208m* (d) 225m

Last Answer : (c) 208m*