Paint Zinc chromate Red oxide primer confirms to IS

1 Answer

Answer :

2074

Related questions

Description : Paint Zinc chromate primer confirms to IS

Last Answer : 104

Description : In areas where there is severe corrosion Finishing coat will be a) Two coats of aluminium paint to IS : 2339* b) One coat of zinc chromate priming to IS : 104 e) Two cover coats of red oxide paint to IS :123 f) One coat of zinc chrome - red oxide priming to IS : 2074

Last Answer : a) Two coats of aluminium paint to IS : 2339*

Description : In areas where there is no severe corrosion Finishing coat will be a) Two coats of aluminium paint to IS : 2339 b) One coat of zinc chromate priming to IS : 104 c) Two cover coats of red oxide paint to IS :123* d) One coat of zinc chrome - red oxide priming to IS : 2074

Last Answer : c) Two cover coats of red oxide paint to IS :123*

Description : aint Red Oxide confirms to IS

Last Answer : 123

Description : Paint Aluminium confirms to IS

Last Answer : 2339

Description : Putty is made up of a) White lead and turpentine b) Powdered chalk and raw linseed oil* c) Red lead and linseed oil d) Zinc oxide and boiled linseed oil

Last Answer : b) Powdered chalk and raw linseed oil*

Description : Shelf life of Paint Red Oxide Ready mixed (IS : 123) a) 4 month b) 1 year* c) 6 month d) None of the above

Last Answer : b) 1 year*

Description : While painting with red oxide paint, a little quantity of ………..shall be added to the paint while doing the first coat to distinguish it from the second coat a) little blue paint b) lamp black* c) red paint d) green paint

Last Answer : b) lamp black*

Description : The maximum time lag between the primer coat and the Ist finishing coat shall not exceed a) 3 days b) 7 days* c) 4 days d) 12 days

Last Answer : b) 7 days*

Description : The maximum time lag between surface preparation and the application of primer coat shall not exceed a) 12 hours b) 24 hours* c) 48 hours d) 36 hours

Last Answer : b) 24 hours*

Description : While painting with Aluminium paint, a little quantity of ………..shall be added to the paint while doing the first coat to distinguish it from the second coat a) little blue paint* b) lamp black c) red paint d) green paint

Last Answer : a) little blue paint*

Description : Which of the substances listed should be applied to battery terminals to help prevent corrosion? A. Zinc chromate B. Naval jelly C. Lead peroxide D. Petroleum jelly

Last Answer : Answer: D

Description : What is used as a photocatalyst? a) Titanium dioxide b) Lead chromate c) Cobalt pigments d) Iron oxide

Last Answer : a) Titanium dioxide

Description : Can I use primer on a cardboard box before using acrylic paint? And is using primer/gesso necessary in this situation?

Last Answer : As we advised on your earlier and very similar question, just take some other piece of cardboard and try it out.

Description : How do I stop stains from seeping through paint primer?

Last Answer : Not sure, but I think Kilz (yes, that’s the product name) might work.

Description : Do I need primer before I paint a patch of my wall?

Last Answer : Paint should be fine. Just be prepared for multiple coats.

Description : What makes primer more "sticky" than paint?

Last Answer : My SIL is a painter by trade. He uses regular paint for everything. It's just another coat to him. Any kind of paint will seal an unfinished surface making the second coat glide. The only time he ... primer is when he has to use Kilstain or some other product to stop bleeding from water stains, etc.

Description : Is it necessary to use primer under interior wall paint?

Last Answer : It is not necessary to use a primer for interior walls, but using one helps with adhesion and smoothness of the paint.

Description : Use a Behr Paint and Primer Combo to Cover Exisiting Paint?

Last Answer : Behr paint covers very well, but for only ten dollars more a gallon, you can get Behr's paint and primer in one. If you are covering a dark color, white, painting fresh drywall, wood, or any ... the exact color you want, with Behr's leading paint technology that gets a clear, rich color every time.

Description : Does two in one paint and primer actually work?

Last Answer : Yes, from personal experience two in one paint and primer does work. If you are not sure you can always go to a place like Lowes or Home Depot to get some more answers.

Description : Name the material which is separated from molten steel during chemical reaction of A.T welding? (i) Aluminium oxide (slag). * (ii) Ferrous Oxide (iii) Aluminium (iv) Ferrous

Last Answer : (i) Aluminium oxide (slag). *

Description : Soundness test of cement is done to determine its a) Durability in seawater b) Free lime content* c) Iron oxide content d) Alumina content

Last Answer : b) Free lime content*

Description : Quicklime is a) Calcium carbonate b) Calcium bicarbonate c) Calcium oxide* d) Calcium hydroxide

Last Answer : c) Calcium oxide*

Description : The lime which contains mainly calcium oxide and slacks with water, is known as a) Fat lime b) Quicklime* c) Hydraulic lime d) Poor line

Last Answer : b) Quicklime*

Description : Which one of the following impurity is not desirable in the soil used for brick formation a) Alkali b) Kankar c) Iron oxide d) Alkali & Kankar*

Last Answer : d) Alkali & Kankar*

Description : Name the paint used in A.T. Welding painting? (i) Black Paint (ii) Bituminous black IS:9862-1981.* (iii) Any type of black paint (iv) None of the above

Last Answer : (ii) Bituminous black IS:9862-1981.*

Description : Second coat of paint is done after minim. of (i) 2 Hrs after first coat (ii) 4 Hrs after first coat (i) 6 Hrs after first coat (iv) 8 Hrs. after first coat

Last Answer : (iv) 8 Hrs. after first coat

Description : Shelf life of Paint aluminium when paste and oil are mixed a) Oneday* b) 1 year c) 6 month d) None of the above

Last Answer : a) Oneday*

Description : Paint is the mixture of ……. a) Binder, Pigment & Solvent* b) Binder & Pigment c) Binder & Solvent d) None of the above

Last Answer : a) Binder, Pigment & Solvent*

Description : Elcometer is used to measure the ……….. a) cross level b) Gauge c) Thickness of paint* d) All the above

Last Answer : c) Thickness of paint*

Description : The pigment used in paints for corrosive resistance, is (A) White lead (B) Ferrous oxide (C) Zinc white (D) Red lead

Last Answer : Answer: Option D

Description : Marking of DFWO weld is. (i) Two red point circle on both faces of weld.* (ii) Two red point cross on both faces of weld. (iii) One red point circle on both faces of weld. (iv) None of the above.

Last Answer : i) Two red point circle on both faces of weld.*

Description : Colour of rail ends becomes after preheating ? (i) Golden * (ii) Pink Red (iii) Red (iv) Yellow

Last Answer : (i) Golden

Description : The colour of bag containing Portion for 110 UTS ? (i) Red (ii) Green (iii) Pink (iv) Black*

Last Answer : iv) Black*

Description : he colour of bag containing Portion for 90 UTS ? (i) Red (ii) Green * (iii) Pink (iv) Black

Last Answer : ii) Green *

Description : The colour of bag containing Portion for 72 UTS ? (i) Pink (ii) Green (iii) Red * (iv) Black

Last Answer : (iii) Red *

Description : The danger level should be marked with a bright red band …… wide centrally over a white band …… wide for a length of……… a) 5 cm, 10 cm, 60 cms* b) 10 cm, 20 cm, 60 cm c) 15 cm, 30 mm, 60 cm d) None of the above

Last Answer : a) 5 cm, 10 cm, 60 cms*

Description : What is the trade name of lead chromate ?

Last Answer : The trade name for lead chromate is chrome yellow.

Description : What happen when a solution of potassium chromate is treated with an excess of dil. Nitic acid?

Last Answer : What happen when a solution of potassium chromate is treated with an excess of dil. Nitic acid? A. `Cr^( ... CrO_4^(2-)` is oxidized to +7 state of Cr

Description : What happen when a solution of potassium chromate is treated with an excess of dil. Nitic acid?

Last Answer : What happen when a solution of potassium chromate is treated with an excess of dil. Nitic acid? A. Cr reduces ... (2-)` and `H_(2)O` will be formed.

Description : Why silver nitrate reacts with chloride ions before chromate ions in Mohr's method?

Last Answer : Feel Free to Answer

Description : What is the formula for cobalt (iii) chromate?

Last Answer : The formula for cobalt(III) chromate is Co2(CrO4)3.

Description : Pick out the wrong statement about coating/electroplating of metals. (A) Phosphate coating is used as an excellent base for paints & enamels (B) Phosphate coating is less corrosion resistant than ... coating metal is made the anode (D) Calorising is the process of coating steel with chromium

Last Answer : (D) Calorising is the process of coating steel with chromium

Description : "Official confirms report." "Authorities have been notified." Do you know anyone personally who is an actual "official" or "authority"? Are you one?

Last Answer : answer:I’ve always assumed that “Official” refers to an official officer of the state. “Authorities” are those authorized by the Officials to conduct investigations, make arrests, and enforce law. You know… The Fuzz. Perhaps my assumptions are presumptuous.

Description : A word for when one neither confirms nor deny something?

Last Answer : No contest?

Description : A brain scan confirms: you are straight. But in reality you are gay. How would you react?

Last Answer : I would disregard any brain scan aiming to tell me what sexuality I am.

Description : A ………… confirms to all the XML guidelines. -Technology

Last Answer : well-formed document

Description : A 55 year-old female complaining of vague tiredness is found to have a serum corrected calcium concentration of 2.9 mmol/l. Examination was unremarkable. Which of the following results ... 4) Low normal plasma phosphate concentration 5) Low normal serum 25-hydroxyvitamin D concentration

Last Answer : Answers-3 Bit too easy really. A high or even normal PTH concentration in the presence of hypercalcaemia would support the diagnosis of hyperparathyroidism. A high urinary Calcium concentration may ... but neither confirm the diagnosis. Elevated 1,25 VitD suggests a diagnosis of hypervitaminosis D.

Description : Which one is the incorrect statement with regard to the importance of pedigree analysis? (a) It confirms that DNA is the carrier of genetic information. (b) It helps to understand whether the trait in ... linked to one of the autosome. (d) It helps to trace the inheritance of a specific trait.

Last Answer : (a) It confirms that DNA is the carrier of genetic information.