On inspecting a completed weld which has charpy impact requirements some small, smooth, shallow areas of undercut have been found <0.25mm deep. The welder says he can quickly put this right by depositing a thick narrow bead along the undercut, in this situation what would you?
a) Agree to go ahead with no preheat as the weld is so small
b) Agree to go ahead with the same preheat as the original weld
c) Agree to go ahead with a preheat 50°C above original
d) Only allow the welder to cosmetically blend out the undercut
a) Agree to go ahead with no preheat as the weld is so small
b) Agree to go ahead with the same preheat as the original weld
c) Agree to go ahead with a preheat 50°C above original
d) Only allow the welder to cosmetically blend out the undercut